Name: | TC4 (Ti-6l-4V) Titanium Alloy Sheet |
Alloy: | TC4 (Ti-6l-4V) |
Execution Standards: | GB/T 3621 AMS 4911 ASTM B265 AMS-T-9046 |
Application: | Materials used in aerospace, automotive and new energy, industrial molds and dies, and semiconductor fields |
Company Info. |
JimaFor |
Verified Supplier |
View Contact Details |
Product List |
Unique Advantages | Main Applications | Execution Standards |
1. Excellent corrosion resistance | 1. Medical components | GB/T 3621 |
2. Excellent fatigue strength | 2. Chemical components | AMS 4911 |
3. Good machinability | 3. Marine components | ASTM B265 |
4. Good strength-to-weight ratio | 4. Racing components | AMS-T-9046 |
Element | Ti | Al | V | Fe | C | N | H | O | Other Single | Other Total |
Min | Balance | 5.5 | 3.5 | | | | | | | |
Max | Balance | 6.75 | 4.5 | 0.3 | 0.08 | 0.05 | 0.015 | 0.2 | 0.1 | 0.4 |
Room - Temperature Tensile Properties | High - Temperature Mechanical Properties | |||
| Minimum | | Minimum | Minimum |
Tensile Strength (Rm)/MPa | 895 | Tensile Strength (Rm)/MPa | 590 | 440 |
Yield Strength (Rp0.2)/MPa | 825 | Test Stress (σ)/MPa | 540 | 195 |
Elongation after Fracture (A)/% | 9 | Test Time (t)/h | 100 | 100 |
Reduction of Area (Z)/% | - | Test Temperature/℃ | 400 | 500 |
Alloy | Condition | Thickness Range/mm | Tensile Strength (Rm)/MPa | Yield Strength (Rp0.2)/MPa | Elongation after Fracture /% ≥ | Bending Radius |
TA2 | M | 0.3 - 1.0 | 440 - 620 | ≥320 | ≥35 | ≥100°, 3t |
| | > 1.0 - 2.0 | 440 - 620 | ≥320 | ≥30 | ≥100°, 3t |
| | > 2 - 5.0 | 440 - 620 | ≥320 | ≥25 | ≥90°, 3t |
| | > 5 - 10.0 | 440 - 620 | ≥320 | ≥25 | - |
| | > 10.0 - 30 | 440 - 620 | ≥320 | ≥18 | - |
TC4 | M | 0.5 - 1.8 | 925 - 1150 | ≥870 | ≥12 | ≥105°, 9t |
| | > 1.8 - 4.0 | 925 - 1150 | ≥870 | ≥12 | ≥105°, 10t |
| | > 4.0 - 5.0 | 925 - 1150 | ≥870 | ≥10 | ≥105°, 10t |
| | > 5.0 - 10.0 | 925 - 1150 | ≥825 | ≥10 | - |
| | > 10.0 - 100 | 925 - 1150 | ≥825 | ≥9 | - |
Alloy | Condition | Thickness Range/mm | Tensile Strength (Rm)/MPa | Test Temperature/℃ | Test Stress(σ)/MPa | Test Time(t)/h |
TC4 | M | 0.5 - 30.0mm | ≥590 | 400 | 540 | ≥100 |
| | | ≥540 | 500 | 195 |
![]() |