Sign In | Join Free | My ecer.jp |
|
Categories | Monel Alloy |
---|---|
Brand Name: | TSING SHAN |
Model Number: | Monel Alloy K500 |
Certification: | ISO MTC SGS |
Place of Origin: | China |
MOQ: | 100KGS |
Price: | 36.5 USD/KG |
Payment Terms: | L/C, Western Union, T/T |
Supply Ability: | 80000KGS |
Delivery Time: | 7 Days |
Packaging Details: | Wooden Box |
Form Of Supply: | Forging, rod, round bar, tube, strip |
Composition: | Nickel, Molybdenum, Chromium, Iron, Cobalt, Tungsten |
Technique: | Cold-rolled |
Equal Grade: | Monel Alloy K500 |
Packing: | standard export packing |
Product: | Monel Alloy K500 Round Bar |
Company Info. |
TSING SHAN STEEL INDUSTRIAL LIMITED |
Verified Supplier |
View Contact Details |
Product List |
Nickel Alloy Monel K500 | UNS# N05500 is an age hardenable
nickel-copper alloy that demonstrates excellent corrosion
resistance, good strength and hardness, mostly resistant to
sour-gas environments, is nonmagnetic, and is superior to Alloy
400. Monel K500 also has great mechanical properties in sub-zero
temperatures and can be found in applications that include valve
components for ships, offshore drilling, oil well collars,
centrifugal pumps, impellers, and other similar
Nickel Alloy Monel K500 Specifications:
DISCLAIMER: Alloy data sheets are for reference only, not for design purposes.
CHEMICAL COMPOSITION | |||||||||
---|---|---|---|---|---|---|---|---|---|
Ni 63.0% Max | Cu 27 – 33.0% | Al 2.30 – 3.15% | Fe 2.0% Max | Mn 0.20% Max | |||||
Ti 0.35 – 0.85% | Si 0.50% Max | C 0.25% Max | S 01% Max |
PHYSICAL PROPERTIES | ||||||
---|---|---|---|---|---|---|
Density | Electrical conductivity (% IACS) | Thermal conductivity (BTU-in/hr-ft²-°F) | Specific heat capacity | Thermal expansion (1/°F) | Melting Point (°F) | |
0.3054 | – | 302 | 0.186 | 0.0000076 | 2460 |
Process | Diameter | Voltage | Amperage | Gas |
TIG | .045" (1.2mm) | 13-16 | 80-110 | 100% Argon |
1/16" (1.6mm) | 14-18 | 90-130 | 100% Argon | |
3/32" (2.4mm) | 15-20 | 120-175 | 100% Argon | |
1/8" (3.2mm) | 15-20 | 150-220 | 100% Argon | |
MIG | .045" (1.2mm) | 28-32 | 180-220 | 75% Argon + 25% Helium |
1/16" (1.6mm) | 29-33 | 200-250 | 75% Argon + 25% Helium | |
SAW | 3/32" (2.4mm) | 28-30 | 275-350 | Suitable Flux may be used |
1/8" (3.2mm) | 29-32 | 350-450 | Suitable Flux may be used | |
5/32" (4.0mm) | 30-33 | 400-550 | Suitable Flux may be used |
Hastelloy | Density g/cm3 | Melting point ºC | Elongation A5 % | Tensile Strength Rm N/mm2 | Yield Strength RP0.2N/mm2 |
C-276 | 8.9 | 1325-1370ºC | 62 | 758 | 363 |
C-22 | 8.9 | 1325-1370 ºC | 40 | 690 | 283 |
C-2000 | 8.5 | 1399ºC 2550°F | 45 | 690 | 283 |
B-2 | 9.2 | 1330-1380ºC | 40 | 745 | 325 |
B-3 | 9.22 | 1370-1418ºC | 40 | 760 | 350 |
G-30 | 8.22 | 1399ºC 2550°F | 62 | 524 | 200 |
X | 8.3 | 1260-1355ºC | 30 | 690 | / |
C-4 | 8.64 | 399°C 2550°F | 40 | 690 | 280 |
G-35 | 8.22 | 1370-1400ºC | / | / | / |
C | 8.94 | 1330-1380 ºC | 40 | 690 | 310 |
![]() |